Journal · Production · 09/11/2026
Coating Adhesion 4B on Cement and Tempered Glass (ASTM D3359)
Our protective coating was cross-cut and tape-tested by Eurofins on two bases — cement and tempered glass. Both passed with grade 4B.

A beautiful stone pattern only lasts if the coating protecting it stays bonded to the surface. Once a coating starts to lift, water gets underneath, and peeling follows. That is why adhesion is one of the first things we test.


How adhesion is tested
Eurofins Consumer Product Testing Vietnam used ASTM D3359-22, the cross-cut tape test. A blade cuts a fine grid through the coating down to the base, a pressure-sensitive tape is pressed onto the grid and pulled off, and the grid is rated from 0B (most of the coating removed) to 5B (nothing removed).
Two bases, the same result
- Cement with printed stone-grain finish — Pass, grade 4B (report EFUZ26094616-CG-01)
- Tempered glass with printed stone-grain pattern — Pass, grade 4B (report EFUZ26094740-CG-01)
Grade 4B means only small flakes came away at the cut intersections, affecting less than 5% of the area. Smooth tempered glass is one of the hardest bases for a coating to grip, so reaching 4B on glass as well as on cement shows the bond works across our product range.
Why it matters in demanding conditions
Humid and rainy climates: rain, humidity and condensation constantly look for a way under the coating. A strong bond keeps moisture out of the cement and away from the print.
Hot, sunny climates: daily heat makes surfaces expand and contract, and dust or sand means tables are wiped often. A coating that holds firmly is less likely to chip at edges or wear through where hands and cleaning cloths pass every day.
Heavy commercial use: the same applies indoors in hotels, restaurants and cafés, where tables are cleaned many times a day.
Lab results and everyday production
The reports apply to the samples tested. In production, surfaces are checked before packing as part of our quality control, and products carry a 2-year warranty.
See all four lab reports on our Quality & Compliance page, or request a sample to test the surface yourself.